It forms a thin and strong supeprhydrophilic antifouling coating film, which exhibits superior stain inhibition property (self-cleaning effect). In addition, as its refractive index is low, transparency of glasses will increase.
Its viscosity is low, so it can be easily applied with a sponge or by spraying.
As it is a polysilicate inorganic coating agent, its hard coating film with superior weather resistance will continues to deliver maximum performance.
When coated, silanol group will be formed to create a supeprhydrophilic silica film, and all the dirt on the film will get washed off when it rains.
By thinly coating a material with low refractive index, it improves transparency.
Protection of base material and antifouling effect based on self-cleaning and antistatic properties.
By applying it on the outside of the window panels, it protect them against dirt, and as a result cleaning frequency will be reduced.
Maintains and improves light transmissibility through protection against dirt and low refractive index.
Improvement of transparency based on its hydrophilic property, and antifouling effect that lasts for a long time.
Antifog effect based on super supeprhydrophilic property.
Outdoor weathering test of painted plates.
Left….coated, right….uncoated.
Antifouling effect on window glass
Left….coated, right….uncoated.
Item name | 400mm | 500mm | 600mm | 700mm | 800mm |
Uncoated cover glass | 91.3% | 91.6% | 91.5% | 91.0% | 90.4% |
Coated cover glass | 92.1% | 92.8% | 93.0% | 92.8% | 92.4% |
Item name | 400mm | 500mm | 600mm |
---|---|---|---|
Uncoated cover glass |
91.3% | 91.6% | 91.5% |
Coated cover glass |
92.1% | 92.8% | 93.0% |
Item name | 700mm | 800mm | |
Uncoated cover glass |
91.0% | 90.4% | |
Coated cover glass |
92.8% | 92.4% |
Coating agent: Hydrophilic coating agent
Film thickness: Dry film thickness 0.3µm.
Measuring equipment: UV/VIS spectrophotometer V530 (by JASCO Corporation)
Note: “-“ indicates “unmeasurable” by contact angle gauge.
Item name | Before test | 24 hours | 48 hours | 72 hours | 96 hours | 120 hours |
Uncoated cover glass | 50.6 | 46.3 | 40.7 | 38.2 | 36.6 | 35.5 |
Coated cover glass | ― | ― | 2.5 | 3.0 | 5.3 | 5.0 |
Item name | Before test | 24 hours | 48 hours |
---|---|---|---|
Uncoated cover glass | 50.6 | 46.3 | 40.7 |
Coated cover glass | – | – | 2.5 |
72 hours | 96 hours | 12 hours | |
Uncoated cover glass | 38.2 | 36.6 | 35.5 |
Coated cover glass | 3.0 | 5.3 | 5.0 |
Showered 4,000 ml/cm3 per hour, which is equal to 4,000mm hourly precipitation. This is almost equivalent to yearly amount of rainfall in Osaka.
24 hours (1 day) of showering equals to 24 years of rainfall.
The transition of the contact angle of the coated solar cell cover glass is indicated above.